本研究探讨了自固化大块填充修复系统(STELA,SDI)的微拉伸粘接强度(µTBS)及失败模式,并将其与光固化大块填充修复系统和传统光固化修复系统在人工唾液中短期和长期老化后的表现进行比较。将48颗人牙随机分为三组(n=16):G1组,自固化大块填充修复系统;G2组,光固化大块填充修复系统;G3组,传统光固化修复系统分层充填。完整修复后的牙齿在人工唾液中储存24小时或18个月(每种条件n=8),仅在完成相应老化期后才进行切割,以获得五个梁状试件(约0.9 mm²)。以牙齿作为实验单位。试件储存24小时或18个月(每种条件n=8)。以1 mm/min的横梁速度评估µTBS,使用立体显微镜确定失败模式,并对代表性样本进行扫描电子显微镜分析。数据采用双因素方差分析和Tukey事后检验(α=0.05)。粘接强度受修复系统和老化时间的显著影响(p<0.001)。同时检测到修复系统与老化条件之间存在显著交互作用(p<0.001)。G2组表现出最低的µTBS值和较高的粘接失败发生率。相比之下,G1组的粘接强度与G3组相当,且显著高于G2组。G1组和G3组以 cohesive 失败为主,而G2组粘接失败更为常见。在本体外研究的局限性范围内,自固化大块填充修复系统在制造商推荐的各自粘接策略下,表现出与传统修复系统相似的粘接性能,并在老化后保持了其相对行为。

Abstract

The microtensile bond strength (µTBS) and failure patterns of a self-curing bulk-fill restorative system (STELA, SDI) were investigated and compared with those of a light-cured bulk-fill and a conventional light-cured restorative system following short- and long-term aging in artificial saliva. Forty-eight human teeth were randomly assigned to three groups (n = 16): G1, self-curing bulk-fill restorative system; G2, light-cured bulk-fill restorative system; and G3, conventional light-cured restorative system applied incrementally. Intact restored teeth were stored in artificial saliva for either 24 h or 18 months (n = 8 per condition) and were sectioned only after completion of the respective aging period to obtain five beam-shaped specimens (≈ 0.9 mm²). The tooth was considered the experimental unit. Specimens were stored for either 24 h or 18 months (n = 8 per condition). µTBS was assessed at a crosshead speed of 1 mm/min, and failure modes were determined using stereomicroscopy, with representative samples analyzed by scanning electron microscopy. Data were subjected to two-way ANOVA and Tukey's post hoc test (α = 0.05). Bond strength was significantly influenced by both restorative system and aging time (p < 0.001). A significant interaction between restorative system and aging condition was also detected (p < 0.001). G2 exhibited the lowest µTBS values and a higher prevalence of adhesive failures. In contrast, G1 showed bond strength comparable to G3 and significantly higher than G2. Cohesive failures predominated in G1 and G3, whereas adhesive failures were more frequent in G2. Within the limitations of this in vitro study, the self-curing bulk-fill restorative system demonstrated adhesive performance similar to the conventional restorative system and preserved its relative behavior after aging, under the respective adhesive strategies recommended by the manufacturers.

如何引用

AMA

Larissa Fiorin Arruda, Diana Moreira Gomes Martins, Luan Júlio Ruiz da Silva, Max Pinto da Costa da Rocha, Milton Carlos Kuga, Cristiane de Melo Alencar. Bond strength performance of a self-curing bulk-fill restorative system and light-cured restorative systems after aging: an in vitro study.. Odontology. 2026; doi:10.1007/s10266-026-01540-y.

APA

Larissa Fiorin Arruda, Diana Moreira Gomes Martins, Luan Júlio Ruiz da Silva, Max Pinto da Costa da Rocha, Milton Carlos Kuga, Cristiane de Melo Alencar (2026). Bond strength performance of a self-curing bulk-fill restorative system and light-cured restorative systems after aging: an in vitro study.. Odontology. https://doi.org/10.1007/s10266-026-01540-y

GB/T 7714

Larissa Fiorin Arruda, Diana Moreira Gomes Martins, Luan Júlio Ruiz da Silva, Max Pinto da Costa da Rocha, Milton Carlos Kuga, Cristiane de Melo Alencar. Bond strength performance of a self-curing bulk-fill restorative system and light-cured restorative systems after aging: an in vitro study.[J]. Odontology, 2026 doi:10.1007/s10266-026-01540-y.

在 PubMed增强版 阅读全文

翻译全文 · AI 文献问答 · PDF 原文下载 · 引用导出

获取 PDF 原文 在 PubMed增强版打开 PubMed 原文 DOI

Odontology 的其他文献