评估木质素/PBAT复合材料的生物降解:重量损失和矿化的比较研究

Assessing the Biodegradation of Lignin/PBAT Composites: A Comparative Study of Weight Loss and Mineralization.

获取 PDF 原文 在 PubMed增强版打开

摘要(中文译文)

木质素是一种有前景的聚己二酸-对苯二甲酸丁二醇酯(PBAT)生物基填料,但其对生物降解的真实贡献仍不明确——多数研究仅依赖重量损失,忽视了CO矿化和木质素的抗菌活性。本研究在堆肥条件下,采用重量损失和矿化率两种指标评估了含1 wt%(LP-1)和3 wt%(LP-2)木质素的木质素/PBAT复合材料。木质素表现出双重作用:它促进水解重量损失(40天时LP-1和LP-2分别为18.3%和28.6%),但显著抑制最终矿化(一年矿化率:纯PBAT为65.71%,LP-1和LP-2分别为48.74%和29.53%)。初始矿化速率为负值,表明释放的酚类化合物具有瞬时抗菌活性。木质素提高了结晶温度(48.4 → 92.6 °C)和(-28.5 → 49.1 °C),1%的添加量基本保持了力学性能。这些发现表明,仅凭重量损失不足以评估降解,必须纳入矿化指标。适当的木质素添加量可实现性能与降解可控性的平衡,为绿色复合材料的生命周期评估提供了新见解。

Abstract

Lignin is a promising bio-based filler for poly(butylene adipate-co-terephthalate) (PBAT), yet its true contribution to biodegradation remains unclear-most studies rely on weight loss alone, neglecting CO mineralization and lignin's antibacterial activity. Here, lignin/PBAT composites with 1 wt% (LP-1) and 3 wt% (LP-2) lignin are assessed under composting conditions using both weight loss and mineralization rate. Lignin exhibits a dual role: it promotes hydrolytic weight loss (18.3% and 28.6% for LP-1 and LP-2 at 40 days), but significantly inhibits ultimate mineralization (one-year mineralization: 65.71% for pure PBAT vs. 48.74% and 29.53% for LP-1 and LP-2). A negative initial mineralization rate suggests transient antibacterial activity from released phenolic compounds. Lignin increases crystallization temperature (48.4 → 92.6 °C) and (-28.5 → 49.1 °C), with 1% loading largely preserving mechanical properties. These findings demonstrate that weight loss alone is insufficient to assess degradation; mineralization must be included. Appropriate lignin loading enables balanced performance and degradation controllability, offering new insights into lifecycle assessment of green composites.

如何引用

AMA

Yanyan Dong, Shaochuang Su, Hong Yang, Zixi Han, Dan Huang, Xiaoshuai Han, et al. Assessing the Biodegradation of Lignin/PBAT Composites: A Comparative Study of Weight Loss and Mineralization.. Polymers. 2026; doi:10.3390/polym18162010.

APA

Yanyan Dong, Shaochuang Su, Hong Yang, Zixi Han, Dan Huang, Xiaoshuai Han, et al (2026). Assessing the Biodegradation of Lignin/PBAT Composites: A Comparative Study of Weight Loss and Mineralization.. Polymers. https://doi.org/10.3390/polym18162010

GB/T 7714

Yanyan Dong, Shaochuang Su, Hong Yang, Zixi Han, Dan Huang, Xiaoshuai Han, et al. Assessing the Biodegradation of Lignin/PBAT Composites: A Comparative Study of Weight Loss and Mineralization.[J]. Polymers, 2026 doi:10.3390/polym18162010.

在 PubMed增强版 阅读全文

翻译全文 · AI 文献问答 · PDF 原文下载 · 引用导出

获取 PDF 原文 在 PubMed增强版打开 PubMed 原文 DOI

Polymers 的其他文献