基于DIC的玄武岩纤维增强沙漠砂高强混凝土力学性能与裂纹演化研究

Study on Mechanical Properties and Crack Evolution of Basalt Fiber-Reinforced Desert Sand High-Strength Concrete Based on DIC.

获取 PDF 原文 在 PubMed增强版打开

摘要(中文译文)

本研究探讨了玄武岩纤维增强沙漠砂高强混凝土的强度发展、裂缝演化及增韧机理。首先采用L9(3)正交设计对基准配合比进行优化,随后掺入体积分数为0、0.3%、0.4%和0.5%的玄武岩纤维。结合力学试验、数字图像相关技术、扫描电镜、X射线衍射、热重分析及傅里叶变换红外光谱,阐明纤维掺量、裂缝扩展与微观结构增强机制之间的关系。优化后的基体配合比为水胶比0.32、沙漠砂替代率40%、粉煤灰掺量20%。玄武岩纤维的掺入对28 d抗压强度影响较小,而劈裂抗拉强度显著提高。0.4%纤维组的劈裂抗拉强度最高,达5.46 MPa,较基准配合比提高12.81%。数字图像相关结果表明,玄武岩纤维减少了应变局部化并限制了裂缝张开。0.5%组裂缝开口位移最小,而0.4%组在抗拉强度、应变重分布与裂缝张开控制之间表现出更好的平衡。扫描电镜观察显示,断裂区域附近存在纤维桥接及纤维-基体相互作用。同时,X射线衍射、热重-微商热重及傅里叶变换红外光谱结果显示,主要物相和官能团无明显变化,表明性能提升主要与玄武岩纤维的物理控裂效应有关,而非基体的化学改性。总体而言,0.4%玄武岩纤维被确定为该体系的最佳掺量。

Abstract

This study investigates the strength development, crack evolution and toughening mechanism of basalt fiber-reinforced desert sand high-strength concrete. An L9(3) orthogonal design was first used to optimize the reference mixture, after which basalt fibers with volume fractions of 0, 0.3%, 0.4% and 0.5% were incorporated. Mechanical testing, digital image correlation, SEM, XRD, TG and FTIR were combined to clarify the relationship among fiber dosage, crack propagation and microstructural reinforcement mechanisms. The optimized matrix mixture was obtained with a water-to-binder ratio of 0.32, a desert sand replacement ratio of 40% and a fly ash content of 20%. The incorporation of basalt fiber had little influence on the 28 d compressive strength, whereas the splitting tensile strength was markedly improved. The highest splitting tensile strength was observed in the 0.4% fiber group, reaching 5.46 MPa, which was 12.81% higher than that of the reference mixture. DIC results showed that basalt fiber reduced strain localization and limited crack opening. The 0.5% group had the lowest COD, while the 0.4% group showed a better balance among tensile strength, strain redistribution and crack-opening control. SEM observations showed fiber bridging and fiber-matrix interaction near the fracture region. Meanwhile, XRD, TG-DTG and FTIR showed no obvious changes in the main phases or functional groups, indicating that the improvement was mainly related to the physical crack-control effect of basalt fibers rather than chemical modification of the matrix. Overall, 0.4% basalt fiber was identified as the preferred dosage for the present system.

如何引用

AMA

Pengyu Wang, Qiaoxia An, Lingyan Xu, Junwen Wan, Rui Yin. Study on Mechanical Properties and Crack Evolution of Basalt Fiber-Reinforced Desert Sand High-Strength Concrete Based on DIC.. Materials (Basel, Switzerland). 2026; doi:10.3390/ma19163486.

APA

Pengyu Wang, Qiaoxia An, Lingyan Xu, Junwen Wan, Rui Yin (2026). Study on Mechanical Properties and Crack Evolution of Basalt Fiber-Reinforced Desert Sand High-Strength Concrete Based on DIC.. Materials (Basel, Switzerland). https://doi.org/10.3390/ma19163486

GB/T 7714

Pengyu Wang, Qiaoxia An, Lingyan Xu, Junwen Wan, Rui Yin. Study on Mechanical Properties and Crack Evolution of Basalt Fiber-Reinforced Desert Sand High-Strength Concrete Based on DIC.[J]. Materials (Basel, Switzerland), 2026 doi:10.3390/ma19163486.

在 PubMed增强版 阅读全文

翻译全文 · AI 文献问答 · PDF 原文下载 · 引用导出

获取 PDF 原文 在 PubMed增强版打开 PubMed 原文 DOI

Materials (Basel, Switzerland) 的其他文献