不同粘度的Giomer基复合材料在侵蚀条件下与牙本质的粘结强度

Bond strength of different viscosities Giomer-based composites to dentin under erosive conditions.

获取 PDF 原文 在 PubMed增强版打开

摘要(中文译文)

本研究旨在评估不同黏度的Giomer基修复复合树脂在不同酸蚀条件下与牙本质粘接的粘接强度。选取120个来自人类健康磨牙的牙本质标本,根据酸蚀挑战分为三组:ERO组(初始酸蚀,0.3%柠檬酸,pH 2.6,5分钟,每天5次,持续1天)、CYC组(ERO方案,修复后再进行额外5天的酸蚀循环挑战)和CON组(健康牙本质,无酸蚀,对照组)。标本进一步根据所使用的Giomer基修复材料分为四个亚组(每组10个):流动型复合树脂(FC)、流动型大块填充复合树脂(FBF)、常规黏度复合树脂(CC)和常规黏度大块填充复合树脂(CBF)。在应用两步自酸蚀粘接系统后,在每个样本中制作两个含各组树脂的圆柱体(直径1.5 mm)。在CYC组中,酸蚀循环在放置粘接系统和复合树脂圆柱体之前及之后进行。通过微剪切测试评估粘接强度,并在体视显微镜下对失败模式进行定量分析。数据采用双因素方差分析,随后进行Tukey检验(α < 0.05)。结果显示,酸蚀底物(p = 0.010)和复合树脂(p = 0.037)之间存在显著差异,但二者的交互作用不显著(p = 0.677)。CYC组的粘接强度值低于对照组,且仅FC复合树脂的粘接强度值低于FBF,而CC和CBF之间数值相似。酸蚀循环降低了所有测试复合树脂的粘接强度,与其黏度无关。对于流动型复合树脂,大块填充型的粘接强度值高于传统非大块填充型,而常规黏度复合树脂之间未观察到这一差异。

Abstract

The present study aimed to evaluate the bond strength of Giomer-based restorative composites with different viscosities bonded to dentin under various erosive conditions. One hundred and twenty dentin specimens from human sound molars were selected and divided into three groups according to the erosive challenge: ERO (initial erosion with citric acid 0.3%, pH 2.6, 5 min, 5x/day, 1 day), CYC (ERO protocol, followed by an additional 5-day erosive cycling challenge after restoration), and CON (sound dentin, without erosion, control). Specimens were further subdivided into four groups ( = 10) according to the Giomer-based restorative material used: flowable composite (FC), flowable bulk-fill composite (FBF), regular-viscosity composite (CC), and regular-viscosity bulk-fill composite (CBF). Two cylinders (1.5 mm diameter) with the resins from each group were made in each sample, after applying the two-step self-etching adhesive system. In the CYC group, the erosive cycle was carried out before and after placement of the adhesive system and composite cylinders. Bond strength was assessed by the micro shear test, and failure was quantified in a stereomicroscope. The data were submitted to two-way ANOVA, followed by the Tukey test ( < 0.05). Significant differences were observed for the eroded substrate ( = 0.010) and the composite resins ( = 0.037), but not for their interaction ( = 0.677). The CYC groups showed lower bond strength values than control group, and only the FC composite presented lower values than FBF, while CC and CBF showed similar values. Erosive cycling decreased the bond strength for all composites tested, irrespective of their viscosity. Regarding the flowable composites, the bulk fill one presented a higher value than the conventional non-bulk fill, while this difference was not observed for the regular-viscosity composites.

如何引用

AMA

Maria Laura Diniz Pereira, Kusai Baroudi, Apurva Mishra, José Alejandro Castro González, Bruno Silva Neto, Gabriel Florio Cairo, et al. Bond strength of different viscosities Giomer-based composites to dentin under erosive conditions.. Frontiers in dental medicine. 2026; doi:10.3389/fdmed.2026.1844321.

APA

Maria Laura Diniz Pereira, Kusai Baroudi, Apurva Mishra, José Alejandro Castro González, Bruno Silva Neto, Gabriel Florio Cairo, et al (2026). Bond strength of different viscosities Giomer-based composites to dentin under erosive conditions.. Frontiers in dental medicine. https://doi.org/10.3389/fdmed.2026.1844321

GB/T 7714

Maria Laura Diniz Pereira, Kusai Baroudi, Apurva Mishra, José Alejandro Castro González, Bruno Silva Neto, Gabriel Florio Cairo, et al. Bond strength of different viscosities Giomer-based composites to dentin under erosive conditions.[J]. Frontiers in dental medicine, 2026 doi:10.3389/fdmed.2026.1844321.

在 PubMed增强版 阅读全文

翻译全文 · AI 文献问答 · PDF 原文下载 · 引用导出

获取 PDF 原文 在 PubMed增强版打开 PubMed 原文 DOI

Frontiers in dental medicine 的其他文献