摘要(中文译文)

评估转化程度对于评价增材制造牙科甲基丙烯酸酯的加工质量具有重要意义。然而,广泛使用的衰减全反射-傅里叶变换红外光谱(ATR-FTIR)方法基于1637/1608 cm⁻¹比值,在当代甲基丙烯酸酯体系中可能因光谱重叠以及芳香参比谱带的配方依赖性行为而不稳定。本研究评估了一种基于聚合敏感、酯相关谱带对1320/1352 cm⁻¹的低方差ATR-FTIR方案,用于估算两种市售增材制造微填充牙科树脂的表面或近表面转化程度,这两种树脂的基质分别以乙氧基化双酚A二甲基丙烯酸酯(Bis-EMA)和氨基甲酸酯二甲基丙烯酸酯(UDMA)为主。常规1637/1608 cm⁻¹比值作为对比方法平行分析。在制造商推荐的全部加工阶段中,从后固化前的生坯状态到最终后固化状态,1320/1352 cm⁻¹模型产生了化学上合理且统计稳定的转化轨迹。相比之下,常规芳香归一化方法表现出更大的配方和工作流程依赖性,分析稳定性较低。在以UDMA为主的树脂中,光照后固化后转化率从68.44%提高至91.61%。对于以Bis-EMA为主的树脂,同一模型揭示了显著的加工阶段效应,在光照与热处理联合处理后实际平台期接近91%。1320/1352 cm⁻¹方案的变异系数较低(0.54-5.58%),而常规方法为29.13-673.09%,且后者在某些组中还产生了非物理的负值估计。在所测试的条件下,这些发现支持将1320/1352 cm⁻¹ ATR-FTIR工作流程作为所研究的两种材料-工作流程体系表面或近表面表征的实用方法。然而,在更广泛采用之前,仍需针对正交分析方法和性能相关结局开展更广泛的验证。

Abstract

Assessing the degree of conversion is important for evaluating processing quality in additively manufactured dental methacrylates. However, the widely used attenuated total reflectance-Fourier transform infrared (ATR-FTIR) method, based on the 1637/1608 cm⁻¹ ratio, may be unstable in contemporary methacrylate systems because of spectral congestion and the formulation-dependent behaviour of the aromatic reference band. This study evaluated a low-variance ATR-FTIR protocol based on a polymerisation-sensitive, ester-associated band pair at 1320/1352 cm⁻¹ to estimate surface or near-surface conversion in two commercially available microfilled dental resins for additive manufacturing, with matrices dominated by ethoxylated bisphenol A dimethacrylate (Bis-EMA) and urethane dimethacrylate (UDMA). The conventional 1637/1608 cm⁻¹ ratio was analysed in parallel as a comparative method. Across the manufacturer-recommended processing stages, from the green state before postcuring to the final postcured state, the 1320/1352 cm⁻¹ model yielded chemically plausible and statistically stable conversion trajectories. In contrast, the conventional aromatic-normalised method showed greater dependence on formulation and workflow, and lower analytical stability. In the UDMA-dominant resin, conversion increased from 68.44% to 91.61% after light postcuring. For the Bis-EMA-dominant resin, the same model revealed a significant processing-stage effect, with a practical plateau near 91% after combined light and thermal treatment. The coefficients of variation for the 1320/1352 cm⁻¹ protocol were low (0.54-5.58%) compared with those of the conventional method (29.13-673.09%), which also yielded nonphysical negative estimates in some groups. Under the conditions tested, these findings support the 1320/1352 cm⁻¹ ATR-FTIR workflow as a practical approach for surface or near-surface characterisation of the two material-workflow systems studied. However, broader validation against orthogonal analytical methods and performance-related outcomes is needed before wider adoption.

如何引用

AMA

Frank Alifui-Segbaya. ATR-FTIR assessment of degree of conversion across curing-state transitions in Bis-EMA- and UDMA-based microfilled dental resins for additive manufacturing.. Journal of materials science. Materials in medicine. 2026; doi:10.1007/s10856-026-07110-6.

APA

Frank Alifui-Segbaya (2026). ATR-FTIR assessment of degree of conversion across curing-state transitions in Bis-EMA- and UDMA-based microfilled dental resins for additive manufacturing.. Journal of materials science. Materials in medicine. https://doi.org/10.1007/s10856-026-07110-6

GB/T 7714

Frank Alifui-Segbaya. ATR-FTIR assessment of degree of conversion across curing-state transitions in Bis-EMA- and UDMA-based microfilled dental resins for additive manufacturing.[J]. Journal of materials science. Materials in medicine, 2026 doi:10.1007/s10856-026-07110-6.

在 PubMed增强版 阅读全文

翻译全文 · AI 文献问答 · PDF 原文下载 · 引用导出

获取 PDF 原文 在 PubMed增强版打开 PubMed 原文 DOI