{"_":"熔融FLiBe(2LiF-BeF₂)中氢同位素的渗透行为:识别不确定性来源及相关测量挑战。","sub":["2"]}
{"_":"Permeation behaviour of hydrogen isotopes in molten FLiBe (2LiF-BeF): Identifying sources of uncertainty and associated measurement challenges.","sub":["2"]}
{"_":"Permeation behaviour of hydrogen isotopes in molten FLiBe (2LiF-BeF): Identifying sources of uncertainty and associated measurement challenges.","sub":["2"]}
本文介绍了在HYPERION装置中开展的系统性研究结果,旨在量化氢同位素在FLiBe中于773K至973K温度范围内的渗透率。针对早期研究报告的输运参数分散性较大所导致的知识空白,HYPERION实验采取了针对性措施以探究未经证实的假设,包括一维渗透、膜表面被熔盐覆盖以及盐-金属界面的理想润湿性。金属侧充氢条件下同位素输运行为受到抑制,凸显了含气泡的Ni-FLiBe界面的渗透阻挡特性,其对渗透率的影响高达77%。本工作试图通过盐侧充氢来解决这一问题,并为未来研究中渗透物充注方法的约束条件提供依据。HYPERION实验的初步发现对早期工作中的设计选择和估算的输运性质提出了质疑。本研究为FLiBe中H/D/T输运观测到的分散性提供了合理解释。
This paper presents results from systematic investigations conducted in the HYPERION facility to quantify permeabilities of hydrogen isotopes in FLiBe over a temperature range of 773K - 973K. To address the knowledge gap resulting from widely scattered transport parameters reported in the earlier studies, HYPERION experiments incorporate specific provisions to probe unsubstantiated assumptions, including a one-dimensional permeation, membrane surface coverage by the salt, and ideal wettability of the salt-metal interface. Suppression of the isotopic transport behaviour for metal-side charging highlights the permeation barrier characteristics of a bubble-laden Ni-FLiBe interface, impacting permeability by up to 77%. This work attempts to resolve this issue via salt-side charging and informs constraints on the permeant charging methodology for future studies. The initial insights from HYPERION experiments call into question the design choices and estimated transport properties in earlier works. This study provides a plausible explanation for the observed scatter in H/D/T transport in FLiBe.
Abhishek Saraswat, Weiyue Zhou, Nayoung Kim, Jaron F Cota, Guiqiu Zheng, Alexander A Khechfe, et al. {"_":"Permeation behaviour of hydrogen isotopes in molten FLiBe (2LiF-BeF): Identifying sources of uncertainty and associated measurement challenges.","sub":["2"]}. International journal of hydrogen energy. 2026; doi:10.1016/j.ijhydene.2026.156016.
Abhishek Saraswat, Weiyue Zhou, Nayoung Kim, Jaron F Cota, Guiqiu Zheng, Alexander A Khechfe, et al (2026). {"_":"Permeation behaviour of hydrogen isotopes in molten FLiBe (2LiF-BeF): Identifying sources of uncertainty and associated measurement challenges.","sub":["2"]}. International journal of hydrogen energy. https://doi.org/10.1016/j.ijhydene.2026.156016
Abhishek Saraswat, Weiyue Zhou, Nayoung Kim, Jaron F Cota, Guiqiu Zheng, Alexander A Khechfe, et al. {"_":"Permeation behaviour of hydrogen isotopes in molten FLiBe (2LiF-BeF): Identifying sources of uncertainty and associated measurement challenges.","sub":["2"]}[J]. International journal of hydrogen energy, 2026 doi:10.1016/j.ijhydene.2026.156016.