摘要(中文译文)

本研究探讨了聚乙烯基甲基醚-马来酸酐共聚物(PVM/MA)的掺入以及热循环老化对酸蚀-冲洗型粘接剂(Adper Single Bond Plus-ASB)和两种不同自酸蚀粘接系统(Clearfil SE Bond-CSE和Fluorobond II-FLB)与牙本质剪切粘接强度(SBS)的影响。将粘接系统应用于从60颗拔除磨牙咬合面随机选取的240个牙本质切片上。测试分组如下(n=20):(G1)纯Clearfil SE(CSE)粘接剂;(G2)含共聚物的CSE(50 mg/ml PVM/MA);(G3)纯FL II粘接剂(FLB);(G4)含共聚物的FLB(50 mg/ml PVM/MA);(G5)纯Adper Single Bond(ASB);(G6)含共聚物的ASB(50 mg/ml PVM/MA)。将树脂复合物(Clearfil Majesty Posterior)应用于牙本质表面并进行光固化。每组一半试样在制备后立即测试(IM),另一半在经历20,000次热循环(TC;5-55 °C)后测试。以0.5 mm/min的横梁速度测量SBS值。数据采用方差分析和Tukey's HSD检验进行分析。PVM/MA共聚物的掺入改善了IM组中CSE的性能以及TC组中ASB的性能,但对其他粘接剂组无影响。含PVM/MA共聚物的自酸蚀粘接剂CSE在IM组中表现出最高的牙本质表面粘接强度(22.0±1.7 MPa)。然而,共聚物的掺入并未提高含氟粘接剂FLB的粘接性能。除含PVM/MA共聚物的ASB树脂粘接剂外,所有测试组中试样的热循环均显著降低了粘接强度。将PVM/MA掺入乙醇基、亲水性全合一粘接剂中可能为提高粘接系统的长期稳定性提供一种有价值的策略。

Abstract

This study investigated the effect of Polymethyl vinyl ether-co-maleic anhydride (PVM/MA) copolymer incorporation and aging with thermocycling on the shear bond strength (SBS) of an etch-and-rinse adhesive (Adper Single Bond Plus-ASB) and two different self-etch adhesive systems (Clearfil SE Bond-CSE and Fluorobond II-FLB) to dentin. Adhesive systems were applied to 240 dentin sections randomly selected from the occlusal surfaces of 60 extracted molar teeth. The test groups were as follows (n=20): (G1) Pure Clearfil SE (CSE) Bond; (G2) CSE with copolymer (50 mg/ml PVM/MA); (G3) Pure FL II Bond (FLB); (G4) FLB with copolymer (50 mg/ml PVM/MA); (G5) Pure Adper Single Bond (ASB); and (G6) ASB with copolymer (50 mg/ml PVM/MA). A resin composite (Clearfil Majesty Posterior) was applied to the dentin surfaces and light-cured. Half of the specimens from each group were tested immediately after preparation (IM) and the other half was tested after exposure to 20,000 thermal cycles (TC; 5-55 °C). SBS values were measured at a crosshead speed of 0.5 mm/min. Data were analyzed with ANOVA and Tukey's HSD. The PVM/MA copolymer incorporation improved the performance of CSE in the IM group and ASB in the TC group, however, it showed no influence in the other adhesive groups. The self-etch adhesive CSE with the PVM/MA copolymer showed the highest bond strength to dentin surfaces in the IM group (22.0±1.7 MPa). However, copolymer corporation did not increase bonding performance of Fluor containing bonding agent FLB. Thermocycling of test specimens significantly decreased bond strengths in all test groups except for ASB resin adhesive with PVM/MA copolymer. Incorporating PVM/MA into ethanol-based, hydrophilic all-in-one bonding agents may offer a valuable strategy to improve the long-term stability of adhesive systems.

如何引用

AMA

Fusun Ozer, Frances Park, Batu Can Yaman, Zeynep Ozkurt-Kayahan, Francis Mante, Markus B Blatz. Impact of PVM/MA Copolymer on Dentin Bond Durability.. Acta stomatologica Croatica. 2026; doi:10.15644/asc60/2/2.

APA

Fusun Ozer, Frances Park, Batu Can Yaman, Zeynep Ozkurt-Kayahan, Francis Mante, Markus B Blatz (2026). Impact of PVM/MA Copolymer on Dentin Bond Durability.. Acta stomatologica Croatica. https://doi.org/10.15644/asc60/2/2

GB/T 7714

Fusun Ozer, Frances Park, Batu Can Yaman, Zeynep Ozkurt-Kayahan, Francis Mante, Markus B Blatz. Impact of PVM/MA Copolymer on Dentin Bond Durability.[J]. Acta stomatologica Croatica, 2026 doi:10.15644/asc60/2/2.

在 PubMed增强版 阅读全文

翻译全文 · AI 文献问答 · PDF 原文下载 · 引用导出

获取 PDF 原文 在 PubMed增强版打开 PubMed 原文 DOI

Acta stomatologica Croatica 的其他文献