热流耦合作用下玻璃固化炉中气泡管的腐蚀行为
Corrosion Behavior of Bubble Tubes in Glass Curing Furnaces Under the Heat-Flow Coupling Effect.
Corrosion Behavior of Bubble Tubes in Glass Curing Furnaces Under the Heat-Flow Coupling Effect.
在1150 °C高温熔融玻璃环境中,由于气体鼓泡引起的气流对熔体流动的冲刷,玻璃固化炉的鼓泡管长期承受极端热流耦合条件,导致严重腐蚀和结构失效。本文对服役后的Inconel 690鼓泡管进行取样分析,系统研究了其腐蚀形貌、产物分布及腐蚀机理。结果表明,鼓泡管外壁在高温熔融玻璃中发生氧化反应,形成富铬氧化层。然而,在熔融玻璃流冲刷作用下发生局部剥落,导致持续腐蚀。腐蚀行为呈现明显的不对称性。由于氧分压更高且熔融玻璃流速更大,鼓泡流侧(内曲线侧)附近的平均腐蚀速率(0.118 mm/天)显著高于外侧(0.051 mm/天)。揭示了流体冲刷不断去除保护性富铬氧化皮,从而在热流耦合作用下加速氧化-冲蚀循环的协同机理。研究结果为鼓泡管的材料优化和寿命预测提供了实验依据和理论参考。
The bubble tube of a glass curing furnace was subjected to extreme heat-flow coupling conditions for a long time due to the scouring of melt flow caused by the gas flow bubbling in a high-temperature molten glass environment at 1150 °C, resulting in severe corrosion and structural failure. This paper conducts post-service sampling analysis of an Inconel 690 bubble tube, and systematically studies its corrosion morphologies, product distribution and corrosion mechanisms. The results show that the outer wall of the bubble tube undergoes an oxidation reaction in the high-temperature molten glass to form a Cr-rich oxide layer. However, local spalling occurs under the scouring of the molten glass flow, resulting in continuous corrosion. The corrosion behavior shows obvious asymmetry. The average corrosion rate near the bubble flow side (the inner curve side, 0.118 mm/day) is significantly higher than that on the outer side (0.051 mm/day) due to the higher partial pressure of oxygen and greater flow rate of molten glass. It reveals the synergistic mechanism by which fluid scouring continuously removes the protective Cr-rich oxide scale, thereby accelerating the oxidation-erosion cycle under the heat-flow coupling effect. The results provided experimental evidence and theoretical reference for the material optimization and life prediction of bubble tubes.
Heyi Guo, Ce Zheng, Yingjv Li, Qiuyan Huang, Qingbin Zhao, Minhang Sun, et al. Corrosion Behavior of Bubble Tubes in Glass Curing Furnaces Under the Heat-Flow Coupling Effect.. Materials (Basel, Switzerland). 2026; doi:10.3390/ma19112429.
Heyi Guo, Ce Zheng, Yingjv Li, Qiuyan Huang, Qingbin Zhao, Minhang Sun, et al (2026). Corrosion Behavior of Bubble Tubes in Glass Curing Furnaces Under the Heat-Flow Coupling Effect.. Materials (Basel, Switzerland). https://doi.org/10.3390/ma19112429
Heyi Guo, Ce Zheng, Yingjv Li, Qiuyan Huang, Qingbin Zhao, Minhang Sun, et al. Corrosion Behavior of Bubble Tubes in Glass Curing Furnaces Under the Heat-Flow Coupling Effect.[J]. Materials (Basel, Switzerland), 2026 doi:10.3390/ma19112429.